Abstract

An experimental investigation is described into the properties of substitutional indium acceptors in single crystal silicon, concentrating on the production of free holes at low temperatures in p-type samples by the photo-ionization of neutral indium centers, and the subsequent hole capture by ionized indium centers. Electrical transport measurements at thermal equilibrium over the temperature range 77° - 300°K were consistent with description of the indium ground state as six-fold degenerate, with an ionization energy of 0.155 eV at all temperatures. Analysis of the transport measurements permitted a calculation of how the density of capture centers varied with temperature, so that data on "carrier lifetime" from photoconductivity measurements could be expressed as the corresponding capture cross-section. Bridge-shaped samples were prepared of crystals with an indium content of either some 8 x 10^15 or 5 x 10^17 cm^-3, with thicknesses either comparable with or much thinner than the optical penetration depth for extrinsic radiation. The spectral dependence of photoconductive responsivity was measured over the range 0.155 eV to 0.9 eV, and was found to increase above threshold in a manner consistent neither with earlier transmission measurements nor with theoretical models. Carrier lifetime was measured from the strength of low frequency photoconductive response, over the range 70° to 180° K; it was consistent with a hole capture cross-section of some 2 x 10^-13 cm^2 over the 70° - 120° K range, and a steady decrease towar 2 x 10^-15 cm^2 on warming to 180° K. The possible interpretations of apparent structure in the temperature dependence are discussed. In a separate inves~igation reported in an Appendix, the response time of germanium cryogenic thermometers has been measured over the 2° - 50°K range. The response time is 0.03 seconds for a sensor immersed in liquid helium.

Extent

117 p.

Comments

Includes bibliography.|Thesis (M.S.)--Florida Atlantic University, 1967.|FAU Electronic Theses and Dissertations Collection|Charles E. Schmidt College of Science|Includes bibliography.

Identifier

FA00000824

Format

pdf

Share

COinS